MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2205 HF Polyetheretherketone (PEEK), Glass Fiber - High Flow
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D 792
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 3.20 mm
0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 186 MPa27000 psiASTM D 638
Elongation at Break 3.0 %3.0 %ASTM D 638
Tensile Modulus 11.7 GPa1700 ksiASTM D 638
Flexural Strength 283 MPa41000 psiASTM D 790
Flexural Modulus 11.1 GPa1610 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.20 mm
2.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 10.7 J/cm
@Thickness 3.20 mm
20.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D 257
Dielectric Constant 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 19.7 kV/mm500 kV/inShort Term; In Oil; ASTM D 149
Dissipation Factor <= 0.010
@Frequency 1e+6 Hz
<= 0.010
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 3.24 µm/m-°C1.80 µin/in-°FE 831
CTE, linear, Transverse to Flow 50.4 µm/m-°C28.0 µin/in-°FE 831
Deflection Temperature at 1.8 MPa (264 psi) 316 °C600 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 349 - 399 °C660 - 750 °F
Mold Temperature 163 - 218 °C325 - 425 °F
Drying Temperature 149 °C
@Time 10800 sec
300 °F
@Time 3.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
RTP Company RTP 2200 HF TFE 5 Polyetheretherketone (PEEK), PTFE Lubricated - High Flow
VICTREX HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
RTP Company RTP 2203 HF Polyetheretherketone (PEEK), Glass Fiber - High Flow
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone

PQZTA1260 / 159166

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.