MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott IRC-1 Zinc Sulfide Broadband Infrared Ceramic
Categories: Ceramic; Sulfide/Chalcogenide

Material Notes: Zinc Sulfide is suitable material for broadband infrared windows, domes and optics. No other material offers this combination of optical properties and environmental resistance. SCHOTT has developed a ceramic process to produce polycrystalline Zinc Sulfide, IRC-1. IRC-1 has significantly improved optical and mechanical performance compared to CVD processed material.
IRC-1 is the material of choice for mid and long wave IR applications

Advantages:

  • IRC-1 performs with high transmission between 3 – 12 µm
  • Fine grained and homogenous microstructures
    • Higher Strength and Hardness
    • Lower cost finishing
    • Improved results from deterministic finishing
  • Ceramic process allows the production of near net shape dome blanks and curved window blanks
    • Reduces processing time and associated costs
    • Reduces production complexity
    Applications:
    Thermal Imaging Systems
    • Thermography
    • Predictive Maintenance
    • Automotive Safety Systems
    • Vandal Proof Surveillance and Imaging
    • Force Protection
    • Intrinsically Safe IR Imaging Systems

    Machine Vision systems
    • Process Control
    • Robotic Manufacturing: UAV Imaging

    Information provided by SCHOTT.

Key Words: ZnS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.08 g/cc0.147 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 270 - 310270 - 310[kg/mm2]
Modulus of Elasticity 74.0 GPa10700 ksi
Modulus of Rupture 0.120 GPa17.4 ksi
Poissons Ratio 0.270.27
Shear Modulus 29.1 GPa4220 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.90 µm/m-°C
@Temperature -40.0 - 70.0 °C
3.28 µin/in-°F
@Temperature -40.0 - 158 °F
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°F
Thermal Conductivity 16.7 W/m-K116 BTU-in/hr-ft²-°F
 
Optical PropertiesMetricEnglishComments
Refractive Index  2.13
@Wavelength 14000 nm
2.13
@Wavelength 14000 nm
 2.152
@Wavelength 13000 nm
2.152
@Wavelength 13000 nm
 2.17
@Wavelength 12000 nm
2.17
@Wavelength 12000 nm
 2.186
@Wavelength 11000 nm
2.186
@Wavelength 11000 nm
 2.20
@Wavelength 10000 nm
2.20
@Wavelength 10000 nm
 2.212
@Wavelength 9000 nm
2.212
@Wavelength 9000 nm
 2.223
@Wavelength 8000 nm
2.223
@Wavelength 8000 nm
 2.232
@Wavelength 7000 nm
2.232
@Wavelength 7000 nm
 2.239
@Wavelength 6000 nm
2.239
@Wavelength 6000 nm
 2.246
@Wavelength 5000 nm
2.246
@Wavelength 5000 nm
 2.252
@Wavelength 4000 nm
2.252
@Wavelength 4000 nm
 2.257
@Wavelength 3000 nm
2.257
@Wavelength 3000 nm
 2.264
@Wavelength 2000 nm
2.264
@Wavelength 2000 nm
 2.297
@Wavelength 947 nm
2.297
@Wavelength 947 nm
 2.348
@Wavelength 639 nm
2.348
@Wavelength 639 nm
 2.482
@Wavelength 441 nm
2.482
@Wavelength 441 nm
 2.929
@Wavelength 1000 nm
2.929
@Wavelength 1000 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mateck Zinc Sulfide Cleartran (ZnS)
Mateck Zinc Sulphide, ZnS
Schott N-SK4 Glass
Zinc Sulfide, ZnS, Sphalerite (Zincblende)
Germanium, Ge

CSGT9928 / 183181

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.