MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mateck Zinc Sulphide, ZnS
Categories: Ceramic; Sulfide/Chalcogenide; Other Engineering Material; Semiconductor

Material Notes: Semiconductor single crystals. Twins and stacking faults < 4% of hexagonal phase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
a Lattice Constant 5.4093 Å5.4093 Å
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+8 - 1.00e+12 ohm-cm1.00e+8 - 1.00e+12 ohm-cmundoped
Hole Mobility, cm²/V-s 140140
 
Descriptive Properties
Crystal Axis(111)
EPD (cm^-2), MAX500000
Orientation(100); (110); (111)
Orientation Accuracy ( ° ), Max1
Polishingchemical mechanical polishing
 one side or both sides polished
 optical polishing
Production MethodMarkov
Standard Size (mm)10 x 10 x 0.5 or 1
 5 x 5 x 0.5 or 1
Structurecubic
Tolerance of Diameter (mm)0.000 / -0.100
Tolerance of Length (mm)0.05
Tolerance of Thickness (mm)0.05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc Selenide, ZnSe
Zinc Sulfide, ZnS, Wurtzite
Mateck Zinc Selenide, ZnSe
Mateck Zinc Sulfide Cleartran (ZnS)
Zinc Sulfide, ZnS, Sphalerite (Zincblende)

CMAT032 / 87716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.