MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin NEOFLON® EA-LR43 ETFE Pellets  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Modified ETFE, Unreinforced

Material Notes: Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, flaring post-forming processes, and others.

Applications:Bonding material for multilayer coextrusion of Nylon 12 and EP-600 series resin.

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.59 g/cc
@Temperature 25.0 °C
1.59 g/cc
@Temperature 77.0 °F
Bulk Density 0.850 g/cc0.0307 lb/in³
Water Absorption <= 0.10 %
@Thickness 8.50 mm,
Time 86400 sec
<= 0.10 %
@Thickness 0.335 in,
Time 24.0 hour
ASTM D570
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm178 cc-mil/100 in²-24hr-atmat 25°C
Nitrogen Transmission 20.0 cc-mm/m²-24hr-atm50.8 cc-mil/100 in²-24hr-atmat 25°C
Viscosity 1.00e+6 - 1.00e+7 cP
@Temperature 300 - 330 °C
1.00e+6 - 1.00e+7 cP
@Temperature 572 - 626 °F
Melt viscosity
Linear Mold Shrinkage 0.030 - 0.040 cm/cm0.030 - 0.040 in/in
Melt Flow 4.0 - 8.0 g/10 min
@Load 5.00 kg,
Temperature 235 °C
4.0 - 8.0 g/10 min
@Load 11.0 lb,
Temperature 455 °F
Deformation 2.3 %2.3 %13.7 MPa load, at 25°C, 24 hrs; ASTM D621
 5.4 %5.4 %6.7 MPa load, at 100°C, 24 hrs; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
Tensile Strength at Break 40.0 - 50.0 MPa5800 - 7250 psiASTM D638
Elongation at Break 420 - 460 %420 - 460 %ASTM D638
Tensile Modulus 0.490 - 0.784 GPa71.1 - 114 ksiASTM D638
Flexural Modulus 0.882 - 1.372 GPa128 - 199.0 ksiASTM D790
Compressive Strength 11.0 MPa
@Temperature 25.0 °C
1600 psi
@Temperature 77.0 °F
1% deformation; ASTM D695
Izod Impact, Unnotched NBNBASTM D256
Coefficient of Friction 0.055 - 0.0780.055 - 0.078
Coefficient of Friction, Static 0.0600.060Coated-steel surface
Taber Abrasion, mg/1000 Cycles <= 127.2<= 127.29.8 N load, cs-10 wheel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+16 ohm-cm<= 1.00e+16 ohm-cmASTM D257
Dielectric Constant  2.6
@Frequency 1000 Hz
2.6
@Frequency 1000 Hz
ASTM D150
 2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
406 kV/in
@Thickness 0.126 in
Short time; ASTM D149
Dissipation Factor  0.00080
@Frequency 1000 Hz
0.00080
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 - 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
27.8 - 50.0 µin/in-°F
@Temperature 73.4 - 140 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FASTM C177
Melting Point 260 °C500 °F
Maximum Service Temperature, Air 150 °C302 °FContinuous use
Flammability, UL94 V-0V-0
Oxygen Index 31 %31 %ASTM D2863
 
Descriptive Properties
Chemical ResistanceExcellent
Contact Angle96Angle to level
WeatherabilityExcellent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin NEOFLON® RP-4040 EFEP Pellets
BASF Luranyl® KR 2404 Polyphenylene Ether + Styrene-Butadiene Blend
Daikin NEOFLON® EC-6500 ETFE Coating Powder, White
Daikin NEOFLON® EPW-1609BK ETFE Liquid Primer, Black
Daikin NEOFLON® EP-541 Extrusion Grade ETFE

PDAIK125 / 29417

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.