MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin NEOFLON® EPW-1609BK ETFE Liquid Primer, Black
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Description: 10-60 micron thickness.

Processing Methods:Air spray coating.

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oxygen Transmission 70.0 cc-mm/m²-24hr-atm178 cc-mil/100 in²-24hr-atmat 25°C
Nitrogen Transmission 20.0 cc-mm/m²-24hr-atm50.8 cc-mil/100 in²-24hr-atmat 25°C
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.5 - 2.75
@Frequency 1000 Hz
2.5 - 2.75
@Frequency 1000 Hz
ETFE Component; ASTM D150
 2.5 - 2.75
@Frequency 1e+6 Hz
2.5 - 2.75
@Frequency 1e+6 Hz
ETFE Component; ASTM D150
Dissipation Factor 0.00040 - 0.00110.00040 - 0.0011ETFE Component
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0ETFE Component
Oxygen Index 31 %31 %ETFE Component

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin NEOFLON® EA-LR43 ETFE Pellets
Daikin NEOFLON® RP-4040 EFEP Pellets
Daikin NEOFLON® EP-541 Extrusion Grade ETFE
Daikin NEOFLON® EC-6500 ETFE Coating Powder, White

PDAIK077 / 29369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.