MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Special Metals MONEL® 404 Copper-Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Data provided by California Fine Wire and the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 483 MPa70000 psiAnnealed
 655 MPa95000 psiStress relieved
 758 MPa110000 psiHard
Tensile Strength, Yield 172 MPa25000 psiAnnealed
 517 MPa75000 psiStress relieved
 689 MPa100000 psiHard
Modulus of Elasticity 169 GPa24500 ksi
Poissons Ratio 0.2950.295
Shear Modulus 65.0 GPa9430 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000500 ohm-cm0.0000500 ohm-cm
Magnetic Permeability 1.00171.0017200 Oersted; Annealed and Furnace-cooled
 1.00471.0047at 200 Oersted; As-Forged
Curie Temperature <= -85.0 °C<= -121 °FAs-Forged
 <= -79.0 °C<= -110 °FAnnealed and Furnace-cooled
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.3 µm/m-°C
@Temperature 21.0 - 93.0 °C
7.39 µin/in-°F
@Temperature 69.8 - 199 °F
Mean
 15.3 µm/m-°C
@Temperature 21.0 - 300 °C
8.50 µin/in-°F
@Temperature 69.8 - 572 °F
Mean
 16.6 µm/m-°C
@Temperature 21.0 - 538 °C
9.22 µin/in-°F
@Temperature 69.8 - 1000 °F
Mean
 17.6 µm/m-°C
@Temperature 21.0 - 815 °C
9.78 µin/in-°F
@Temperature 69.8 - 1500 °F
Mean
Specific Heat Capacity 0.414 J/g-°C0.0989 BTU/lb-°F
Melting Point 1300 °C2370 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.050 %<= 0.050 %
Carbon, C <= 0.15 %<= 0.15 %
Copper, Cu <= 45.5 %<= 45.5 %As remainder
Iron, Fe <= 0.50 %<= 0.50 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni 52 - 57 %52 - 57 %Including Cobalt
Silicon, Si <= 0.10 %<= 0.10 %
Sulfur, S 0.024 %0.024 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy 400
Special Metals MONEL® Alloy 401
Special Metals MONEL® Alloy R-405
Special Metals MONEL® Alloy K-500
MetalTek MTEK A Cast UNS N04020 Nickel-Copper Alloy

NINCO61 / 17494

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.