MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Live White Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Quercus Virginiana; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.800 g/cc0.800 g/ccGreen, based on volume
 0.880 g/cc0.880 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 10.9 GPa1580 ksiGreen
 13.7 GPa1980 ksi12% moisture content
Modulus of Rupture 0.0820 GPa11.9 ksiGreen
 0.127 GPa18.4 ksi12% moisture content
Compressive Strength 14.1 MPa2040 psiGreen, perpendicular to grain
 19.6 MPa2840 psi12% moisture content, perpendicular to grain
 37.4 MPa5430 psiGreen, parallel to grain
 61.4 MPa8900 psi12% moisture content, parallel to grain
Shear Strength 15.2 MPa2210 psiGreen, parallel to grain
 18.3 MPa2660 psi12% moisture content, parallel to grain
Work to Maximum Load 0.0848 J/cm³12.3 in-lb/in³Green
 0.130 J/cm³18.9 in-lb/in³12% moisture content
 
Thermal PropertiesMetricEnglishComments
Shrinkage 6.6 %6.6 %Radial, from green to oven dry, US origin
 9.5 %9.5 %Tangential, from green to oven dry, US origin
 14.7 %14.7 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Black Ironwood Wood
African Ekki/azobe Wood
American White Oak Wood
Willow Red Oak Wood
Black Red Oak Wood

PTSU040 / 71482

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.