MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F515 Epoxy Resin, BXX120 Carbon Tape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  1572 MPa
@Temperature 23.0 °C
228000 psi
@Temperature 73.4 °F
 1779 MPa
@Temperature 71.0 °C
258000 psi
@Temperature 160 °F
1/2 hr
Tensile Modulus  90.3 GPa
@Temperature 23.0 °C
13100 ksi
@Temperature 73.4 °F
 93.8 GPa
@Temperature 71.0 °C
13600 ksi
@Temperature 160 °F
1/2 hr
Flexural Yield Strength  1172 MPa
@Temperature 71.0 °C
170000 psi
@Temperature 160 °F
1/2 hr
 1372 MPa
@Temperature 23.0 °C
199000 psi
@Temperature 73.4 °F
Flexural Modulus  97.9 GPa
@Temperature 71.0 °C
14200 ksi
@Temperature 160 °F
1/2 hr
 100 GPa
@Temperature 23.0 °C
14500 ksi
@Temperature 73.4 °F
Compressive Yield Strength  1103 MPa
@Temperature 71.0 °C
160000 psi
@Temperature 160 °F
1/2 hr
 1248 MPa
@Temperature 23.0 °C
181000 psi
@Temperature 73.4 °F
Compressive Modulus  90.3 GPa
@Temperature 71.0 °C
13100 ksi
@Temperature 160 °F
1/2 hr
 92.4 GPa
@Temperature 23.0 °C
13400 ksi
@Temperature 73.4 °F
Shear Strength  72.4 MPa
@Temperature 71.0 °C
10500 psi
@Temperature 160 °F
Short Beam, 1/2 hr
 86.9 MPa
@Temperature 23.0 °C
12600 psi
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Carbon/Epoxy Composite Sheet
Goodfellow Carbon/Epoxy Composite Tube
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2
Hexcel® HexPly® ES15 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2

PHEXC129 / 98599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.