MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M21 356°F (180°C) Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® M21 is a new, very tough epoxy matrix that exhibits excellent damage tolerance, especially at high energy impact. It has been developed to meet the needs of the latest generation of primary aircraft structures and Formula 1 Grand Prix cars.
HexPly® M21 benefits from easy processing as a result of controlled flow and a simple cure schedule. It is best suited to press or autoclave cure to obtain optimum mechanical performance from the cured composite.

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Yield Strength 147 MPa21300 psi
Flexural Modulus 3.50 GPa508 ksi
Flexural Strain at Yield 5.0 %5.0 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 185 °C365 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 12.0 Month
@Temperature -18.0 °C
>= 12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Tack Life (days)30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix
Hexcel® HexPly® M10E Epoxy Resin
Hexcel® HexPly® F593 Epoxy Resin

PHEXC162 / 98633

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.