MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: Description:
#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low viscosity, minimum odor and good color. It is designed to be cured with #87 Epoxy Hardener. #87 Epoxy Hardener is a very reactive modified aliphatic amine edduct, developed for applications where relatively short cure periods at room temperature are required. Compositions based on #88 Epoxy Resin and #87 Epoxy Cure readily at room temperature. The pot life of such compositions is highly dependent on the volume of the mixture, temperature, amount and type of filler loading, and, to a lesser extent, the presence of a reactive diluent.

Properties listed determined on 1/8" thick test specimens at 25°C for 16 hours followed by a pot cure of 2 hours at 100°C.

Applications
Adhesives, decoupage systems, thin-set terrazzo flooring and industrial flooring, epoxy crack injection systems, exposed aggregate wall matrix, wet lay-up laminates, high solids/low VOC high performance architectural coatings.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.10 %0.10 %Percent weight gain after 24 hours immersion at 25°C
 0.10 %0.10 %Percent weight loss after 24 hours at 150°C
Viscosity 10000 cP10000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Tensile Strength at Break 75.8 MPa11000 psi
Elongation at Break 3.8 %3.8 %
Flexural Strength 131 MPa19000 psi
Flexural Modulus 3.79 GPa550 ksiInitial flexural modulus
Compressive Yield Strength 111 MPa16100 psi
Izod Impact, Notched 0.246 J/cm0.460 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  6.00e+10 ohm-cm
@Temperature 130 °C
6.00e+10 ohm-cm
@Temperature 266 °F
 8.00e+12 ohm-cm
@Temperature 93.0 °C
8.00e+12 ohm-cm
@Temperature 199 °F
 1.00e+15 ohm-cm
@Temperature 66.0 °C
1.00e+15 ohm-cm
@Temperature 151 °F
 2.80e+16 ohm-cm
@Temperature 25.0 °C
2.80e+16 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 4.194.19
Dissipation Factor 0.026
@Frequency 1e+7 Hz
0.026
@Frequency 1e+7 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 99.0 °C210 °FDeflection Temp; Load not specified
 
Processing PropertiesMetricEnglishComments
Cure Time 240 - 480 min4.00 - 8.00 hourMixture reaches handling strength in 4 to 8 hours.
 5760 - 10080 min96.0 - 168.0 hourFor full cure. Maximum high temperature properties are obtained with a post cure of about 2 hours at 93°C to 121°C.
Pot Life 15.0 min
@Temperature 25.0 °C
15.0 min
@Temperature 77.0 °F
0.25 lb
 
Descriptive Properties
Maximum Exotherm>204°C25 grams, 1 inch thick, at ambient temperature of 25°C and a gel time of 15 minutes.
Mix Ratio100:20Resin:Hardener by Weight

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman Araldite GY 281 Bisphenol F Epoxy Resin
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Solvay CYCOM® 970 Epoxy - Carbon Fiber Reinforced Unidirectional Tape
CHT Group EP QS EPI Engineered Polymers Quick Set Epoxy
DSM Somos® ProtoGen™ 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2

PFIBRE18 / 38290

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.