MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celcon® UV270Z POM, UV Resistant
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Celcon« UV270Z is a nominal 27 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposure. Celcon« UV270Z flow is designed to fill small and difficult to process parts such as speaker grills and other interior automotive parts. The material is available in precolored black or colors.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.75 %0.75 %ISO 62
Linear Mold Shrinkage, Flow 0.017 cm/cm0.017 in/inISO 294-4
 0.022 cm/cm0.022 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4
 0.018 cm/cm0.018 in/inASTM D955
Melt Flow 27 g/10 min27 g/10 minASTM D1238
 23 g/10 min
@Load 2.16 kg,
Temperature 190 °C
23 g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.7 MPa8800 psiASTM D638
 64.0 MPa9280 psi50mm/min; ISO 527-2/1A
Elongation at Yield 8.0 %8.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.70 GPa392 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 2.59 GPa375 ksiASTM D790
 2.76 GPa400 ksiISO 178
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 5.10 kJ/m²2.43 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.470 J/cm²2.24 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-2
Melting Point 165 °C329 °FASTM D3418
 167 °C333 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75-1, -2
 110 °C230 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 180 - 200 °C356 - 392 °Fhot runner
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 190 - 200 °C374 - 392 °F
Die Temperature 190 - 200 °C374 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 4.00 MPa<= 580 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow-medium
PelletsYes
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
Celanese Celcon® UV140LG POM, UV Resistant
Celanese Hostaform® S 27072 WS 10/1570 Elastomer Modified, Weather Resistant Acetal Copolymer
Celanese Celcon® UV90Z POM, UV Resistant
Celanese Celcon® UV25Z POM, UV Resistant

PHCQ143 / 178598

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.