Celcon« UV90Z is an integrally colored nominal 9 melt flow rate based acetal copolymer material stabilized for use where ultraviolet radiation exposure is to be encountered. The material is formulated to prevent discoloration, fading, chalking and mechanical property change in severe ultraviolet exposure. This product is available in many colors formulated for the interior automotive market and other applications.Information provided by Celanese |