MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Avient Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 11.0 g/cc11.0 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.2 MPa3950 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 1.8 %1.8 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8.27 GPa1200 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 48.3 MPa7010 psiASTM D790
Flexural Modulus 4.96 GPa719 ksiASTM D790
Poissons Ratio 0.350.35ASTM E132
Shear Modulus 3.06 GPa444 ksiCalculated
Izod Impact, Notched 1.10 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Unnotched 3.70 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
6.93 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  63.0 µm/m-°C
@Temperature 0.000 - 32.0 °C
35.0 µin/in-°F
@Temperature 32.0 - 89.6 °F
ASTM E831
 100 µm/m-°C
@Temperature 60.0 - 100 °C
55.6 µin/in-°F
@Temperature 140 - 212 °F
ASTM E831
CTE, linear, Transverse to Flow  57.0 µm/m-°C
@Temperature 0.000 - 32.0 °C
31.7 µin/in-°F
@Temperature 32.0 - 89.6 °F
ASTM E831
 84.0 µm/m-°C
@Temperature 60.0 - 100 °C
46.7 µin/in-°F
@Temperature 140 - 212 °F
ASTM E831
Thermal Conductivity 3.50 W/m-K24.3 BTU-in/hr-ft²-°FThe value listed as thermal conductivity, ASTM C177, was tested in accordance with ASTM E1461.; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 6.35 mm
280 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
@Thickness 6.35 mm
190 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 288 °C500 - 550 °F
Mold Temperature 82.2 - 149 °C180 - 300 °F
Drying Temperature 79.4 °C175 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AdditiveImpact Modifier
AppearanceNatural Color
FeaturesHigh Density
 Impact Modified
 Non-Toxic
FormsPellets
Generic MaterialNylon 12
Generic NamePolyamide 12 (Nylon 12)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesIndustrial Applications
 Medical/Healthcare Applications
 Projectiles
 Radiation Shielding
 Sporting Goods
 Weighting & Balancing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PA6 1030
Techmer ES HiFill® PA6 1020
Techmer ES HiFill® TPU 1000
Evonik VESTOSINT® 1101 white Polyamide 12
Evonik VESTAMID® LX9012 PA 12

PH0POL0687 / 145256

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.