System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Chicago Extruded Metals BioBrass® UNS C62400 Aluminum Bronze
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
;
Bronze
Material Notes:
Finished product available as rod or forged.
Chicago Extruded Metal temper codes: H02, M30
This alloy is registered with the U.S. EPA as Antimicrobial.
Information provided by Chicago Extruded Metals
Key Words:
CDA 624, ASTM B150, SAE J461, SAE J463
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
7.45
g/cc
0.269
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell B
87 - 92
87 - 92
Tensile Strength
621
-
724
MPa
90000
-
105000
psi
Tensile Strength, Yield
276
-
359
MPa
40000
-
52000
psi
Elongation at Break
14 - 18 %
14 - 18 %
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.0000144
ohm-cm
0.0000144
ohm-cm
Thermal Properties
Metric
English
Comments
Thermal Conductivity
86.5
W/m-K
600
BTU-in/hr-ft²-°F
Component Elements Properties
Metric
English
Comments
Aluminum, Al
10 - 11.5 %
10 - 11.5 %
Copper, Cu
>= 82.75 %
>= 82.75 %
as balance
Iron, Fe
2.0 - 4.5 %
2.0 - 4.5 %
Manganese, Mn
<= 0.30 %
<= 0.30 %
Other, total
0.50 %
0.50 %
Silicon, Si
<= 0.25 %
<= 0.25 %
Tin, Sn
<= 0.20 %
<= 0.20 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 12.7 - 25.4 mm.
Chicago Extruded Metals BioBrass® UNS C62300 Aluminum Bronze
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 25.4 - 50.8 mm.
NCHICA920 / 147639
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.