MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chicago Extruded Metals BioBrass® UNS C62300 Aluminum Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Finished product available as bar, rod, forged or shapes.
Chicago Extruded Metal temper codes: H02, M30

This alloy is registered with the U.S. EPA as Antimicrobial.

Information provided by Chicago Extruded Metals

Key Words: CDA 623, AMS 4635, ASTM B124, ASTM B150, SAE J461, SAE J463
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.67 g/cc0.277 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 80 - 8980 - 89
Tensile Strength 517 - 676 MPa75000 - 98000 psi
Tensile Strength, Yield 241 - 359 MPa35000 - 52000 psi
Elongation at Break 22 - 35 %22 - 35 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000144 ohm-cm0.0000144 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 86.5 W/m-K600 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.5 - 10 %8.5 - 10 %
Copper, Cu >= 83.15 %>= 83.15 %as balance
Iron, Fe 2.0 - 4.0 %2.0 - 4.0 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni <= 1.0 %<= 1.0 %
Other, total 0.50 %0.50 %
Silicon, Si <= 0.25 %<= 0.25 %
Tin, Sn <= 0.60 %<= 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chicago Extruded Metals BioBrass® UNS C63000 Aluminum Bronze
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze
Medical Grade Stainless Steel 316LVM
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 12.7 - 25.4 mm.

NCHICA919 / 147638

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.