AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether aliphatic polyurethanes designed for use as coatings of catheters, sutures, introducers, rods, valves and rubber products. Hydroslip C polymers can also be coated onto silicon microdevices to reduce absorption of white cells and proteins on the devices, thereby aiding in the analysis of blood and DNA. Information provided by AdvanSource Biomaterials Corporation. |