MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B3L BK00464 PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall plugs.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.1 - 2.9 %2.1 - 2.9 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 8.5 - 9.5 %8.5 - 9.5 %ISO 62
Linear Mold Shrinkage 0.0065 cm/cm0.0065 in/inrestricted
Melt Flow 121 g/10 min
@Load 5.00 kg,
Temperature 275 °C
121 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 18 %18 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 0.900 GPa131 ksiISO 527-1/-2
Izod Impact, Notched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 550 MPa
@Strain <=0.5 %
79800 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 6.4
@Frequency 1e+6 Hz
6.4
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.24
@Frequency 1e+6 Hz
0.24
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°F
Thermal Conductivity 0.320 W/m-K2.22 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °FDIN 53765
Maximum Service Temperature, Air 160 °C320 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °FInjection-molding/Extrusion
Mold Temperature 40.0 - 80.0 °C104 - 176 °FInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Dry)
BASF Ultramid® B33 01 PA6 (Dry)
BASF Ultramid® B32 01 PA6 (Dry)
BASF Ultramid® 8253 PA6 (Conditioned)
BASF Ultramid® 8202 PA6 (Conditioned)

PBASG0254 / 131887

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.