MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8202 PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ultramid 8202 HS) and/or pigmented versions. It combines good strength, stiffness and toughness as well as excellent heat, chemical and abrasion resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³dry; ISO 1183
Melt Density 0.932 g/cc
@Temperature >=220 °C
0.0337 lb/in³
@Temperature >=428 °F
ISO 1183
Water Absorption 1.6 %1.6 %24 hour; ISO Test
 9.5 %9.5 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.7 %2.7 %beginning dry (23°C/50% R.H.); ISO 62
Relative Viscosity 2.6 cP2.6 cPISO Test; 96 % SAV
Viscosity Measurement 4848Formic Acid
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi0.2 in/min; ASTM Test
 80.0 MPa
@Temperature -40.0 °C
11600 psi
@Temperature -40.0 °F
ASTM Test
 80.0 MPa
@Temperature -40.0 °C
11600 psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Yield 36.0 MPa5220 psi50mm/min; ISO 527
 36.0 MPa5220 psi2 in/min; ASTM Test
 20.0 MPa
@Temperature 120 °C
2900 psi
@Temperature 248 °F
ISO Data
 20.0 MPa
@Temperature 120 °C
2900 psi
@Temperature 248 °F
ASTM Test
 30.0 MPa
@Temperature 80.0 °C
4350 psi
@Temperature 176 °F
ASTM Test
 30.0 MPa
@Temperature 80.0 °C
4350 psi
@Temperature 176 °F
ISO Data
 110 MPa
@Temperature -40.0 °C
16000 psi
@Temperature -40.0 °F
ASTM Test
 110 MPa
@Temperature -40.0 °C
16000 psi
@Temperature -40.0 °F
ISO Data
Elongation at Break >= 50 %>= 50 %50mm/min, Nominal strain; ISO 527
 >= 100 %>= 100 %2 in/min; ASTM Test
 2.5 %
@Temperature -40.0 °C
2.5 %
@Temperature -40.0 °F
ASTM Test
 2.5 %
@Temperature -40.0 °C
2.5 %
@Temperature -40.0 °F
ISO Data
Elongation at Yield 16 %16 %50mm/min; ISO 527
 16 %16 %2 in/min; ASTM Test
 35 %
@Temperature 80.0 °C
35 %
@Temperature 176 °F
ASTM Test
 35 %
@Temperature 80.0 °C
35 %
@Temperature 176 °F
ISO Data
 40 %
@Temperature 120 °C
40 %
@Temperature 248 °F
ASTM Test
 40 %
@Temperature 120 °C
40 %
@Temperature 248 °F
ISO Data
Tensile Modulus 0.970 GPa141 ksi1mm/min; ISO 527
 0.320 GPa
@Temperature 120 °C
46.4 ksi
@Temperature 248 °F
ISO Data
 0.550 GPa
@Temperature 80.0 °C
79.8 ksi
@Temperature 176 °F
ISO Data
 4.00 GPa
@Temperature -40.0 °C
580 ksi
@Temperature -40.0 °F
ISO Data
Flexural Strength 25.0 MPa3630 psiISO Data
 35.0 MPa5080 psiASTM Test
 154 MPa
@Temperature -40.0 °C
22300 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 0.740 GPa107 ksiASTM Test
 0.770 GPa112 ksiISO Data
Izod Impact, Notched 0.430 J/cm
@Temperature -40.0 °C
0.806 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM Test
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 3.728 J/g-°C0.8910 BTU/lb-°FMelt
Thermal Conductivity 0.264 W/m-K1.83 BTU-in/hr-ft²-°FMelt
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection molding
Mold Temperature 80.0 °C176 °FInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8202 PA6 (Dry)
Ascend Performance Materials Vydyne® 21SPC Nylon 66, General Purpose
BASF Nypel® 6030G HS BK 30% Glass Filled PA6 (Dry)
BASF Ultramid® 8253 PA6 (Conditioned)
BASF Ultramid® 1000-11 NF2001 PA66 (Conditioned)

PBASF9138 / 84902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.