MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg AEM Syntac® 350 Syntactic Foam
Categories: Polymer; Thermoset; Epoxy

Material Notes: Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.

Available in block, sheet and rod form, Syntac® 350 is easily machined using standard shop tools and offers a lightweight, durable and cost effective alternative to wood, felt and aluminum

All information provided by Trelleborg Emerson & Cuming

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.673 g/cc0.0243 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55
@Temperature 177 °C
55
@Temperature 350 °F
Compressive Strength 44.8 MPa6500 psi
Compressive Modulus 2.34 GPa339 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.6 µm/m-°C17.0 µin/in-°F
Specific Heat Capacity 2.09 J/g-°C0.500 BTU/lb-°F
Thermal Conductivity 0.121 W/m-K0.840 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C350 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg AEM Syntac® 351 Syntactic Foam
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Trelleborg AEM Syntac® Eccolite® Ultra
Trelleborg Emerson & Cuming Eccolite® Composite Materials Ultra Syntactic Foam

PTRELL001 / 83759

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.