Eccolite® Ultra is a new generation syntactic foam plug assist material, a new thermoplastic compound developed in response to the needs of the thermoforming industry. Eccolite® is tough and robust, but also maintains the unique features and benefits of the other products in the Syntac® family. It is manufactured from a specially formulated thermoplastic resin and hollow glass microspheres. Unlike nylon-based materials Eccolite® Ultra boasts an exceptionally high temperature characteristic, maintaining its profile over extended operation cycle terms in service temperatures up to 392°F/200°CAll information provided by Trelleborg Emerson & Cuming |