MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Styroflex® 2G 66 LE Styrene Butadiene Copolymer (SBC)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styroflex® 2G66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE) suitable for extrusion (blown and cast film) and for injection molding. Styroflex® 2G66 is also used for polymers modification and compatibilization. It is more polar than comparable SBS or SEBS grades and offers a combination of high resilience and toughness with good transparency and process stability. Features: Excellent thermostability, Very high elongation at break, High resilience, High transparency, Regulatory compliant, High flow. Applications: Food packaging and films, Stretch hood/ stretch film, Impact modification / ESCR improvement, Compounding, compatibilization, recycling, Medical devices, Adhesives, Soft touch injection molding; toys, 2-K inj. mold.

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.998 g/cc0.0361 lb/in³ISO 1183
Water Absorption at Saturation 0.070 %0.070 %ISO 62
Oxygen Transmission Rate 27.2 cc/m²/day
@Temperature 23.0 °C
1.75 cc/100 in²/day
@Temperature 73.4 °F
0% RH
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
13 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8484ISO 868
Hardness, Shore D 3434ISO 868
Tensile Strength, Yield 4.00 MPa580 psiISO 527
Elongation at Break >= 500 %>= 500 %Nominal; ISO 527
 >= 500 %>= 500 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
Tensile Modulus 0.120 GPa17.4 ksiISO 527
Flexural Strength 4.00 MPa580 psiISO 178
Flexural Modulus 0.140 GPa20.3 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
Elmendorf Tear Strength MD 660 g660 g
Elmendorf Tear Strength TD 816 g816 g
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 35.0 °C
@Load 1.02 kg
95.0 °F
@Load 2.25 lb
B/2 120C/H; ASTM D 1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5651.565Sodium D Line; ISO 489
Haze 5.0 %5.0 %ASTM D 1003
Transmission, Visible 80 %
@Wavelength 550 nm
80 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 240 °C338 - 464 °FISO 294
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °FISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Styroflex® 2G66 SBC
LG Chemical SBR 1502 High Acrylonitrile Polymer
Kraton® D1118 A (SBS) Diblock Copolymer
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer
Dow Engage® ENR 7447.00 Ethylene-Butene Copolymer

PSTYR9881 / 216108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.