MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Styroflex® 2G 66 LE Styrene Butadiene Copolymer (SBC)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styroflex® 2G66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE) suitable for extrusion (blown and cast film) and for injection molding. Styroflex® 2G66 is also used for polymers modification and compatibilization. It is more polar than comparable SBS or SEBS grades and offers a combination of high resilience and toughness with good transparency and process stability. Features: Excellent thermostability, Very high elongation at break, High resilience, High transparency, Regulatory compliant, High flow. Applications: Food packaging and films, Stretch hood/ stretch film, Impact modification / ESCR improvement, Compounding, compatibilization, recycling, Medical devices, Adhesives, Soft touch injection molding; toys, 2-K inj. mold.

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.998 g/ccISO 1183
Water Absorption at Saturation 0.070 %ISO 62
Oxygen Transmission Rate 27.2 cc/m²/day
@Temperature 23.0 °C
0% RH
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84ISO 868
Hardness, Shore D 34ISO 868
Tensile Strength, Yield 4.00 MPaISO 527
Elongation at Break >= 500 %Nominal; ISO 527
 >= 500 %ISO 527
Elongation at Yield 5.0 %ISO 527
Tensile Modulus 120 MPaISO 527
Flexural Strength 4.00 MPaISO 178
Flexural Modulus 140 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Elmendorf Tear Strength MD 660 g
Elmendorf Tear Strength TD 816 g
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 35.0 °C
@Load 1.02 kg
B/2 120C/H; ASTM D 1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.565Sodium D Line; ISO 489
Haze 5.0 %ASTM D 1003
Transmission, Visible 80 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 170 - 240 °CISO 294
Mold Temperature 30.0 - 50.0 °CISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Styroflex® 2G66 SBC
LG Chemical SBR 1502 High Acrylonitrile Polymer
Kraton® D1118 A (SBS) Diblock Copolymer
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer
Dow Engage® ENR 7447.00 Ethylene-Butene Copolymer

PSTYR9881 / 216108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.