MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.

Available in: Europe

Product Applications: TECHNYL A 218W V30 Black FA is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water: i.e. (electro-magnetic valves). This material restricts electrolytical corrosion and can be used as insulation material for electronic connectors. The values of properties are for black grade.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527 Type 1A
Tensile Modulus 7.50 GPa1090 ksiISO 527 Type 1A
Flexural Strength 180 MPa26100 psiISO 178
Flexural Modulus 6.40 GPa928 ksiISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 9.00 J/cm²42.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 3.33.3IEC 60250
Dissipation Factor 0.0800.080IEC 60250
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® B 50 H1 PA66/6, DRY
Domo Technyl® A218 Heat Stabilized Nylon 66

PRHOD679 / 137910

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.