MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Synthos BUNA™ SB 1739 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: BUNA™ SB 1739–Schkopau is manufactured by cold polymerization using mixed rosin acid/fatty acid soaps. In relation to solid rubber it is plasticized with 37.5 parts of TDAE oil which does comply with EU DIRECTIVE 2005/69/EC for use in tires within the EU. A discoloring stabilizer is added during the production process.

Application: BUNA™ SB 1739–Schkopau is a general purpose rubber. It can be processed in all sectors of the tire and rubber industry. The main application is tire production, imparting improved grip and handling performance due to its increased styrene content.

Synthos acquired the synthetic rubber business from Trinseo in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³
Volatiles 0.40 %0.40 %1 hr at 105°C in a hot air oven, 5 g sample; ASTM D5668
Mooney Viscosity 52
@Temperature 100 °C
52
@Temperature 212 °F
MU, ML 1+4; ASTM D1646
Ash 0.040 %0.040 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 40.2 %40.2 %Bound; ASTM D5775
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 23.1 MPa3350 psiCure: 45 min at 145°C; ASTM D412
Elongation at Break 460 %460 %ASTM D412
300% Modulus 14.4 MPa
@Strain 300 %
2090 psi
@Strain 300 %
ASTM D412
 
Descriptive Properties
Organic acid4.3 percentASTM D5774
Rheometer15.6 dNmMH, ASTM D5289
 17.1 mintc(90), ASTM D5289
 2.3 dNmML, ASTM D5289
 5.7 mints2, 160°C, ASTM D5289
 8.4 mintc(50), ASTM D5289
Test Formulation1 PartStearic acid, ASTM D3185-1A
 1 PartAccelerator (TBBS), ASTM D3185-1A
 1.75 PartsSulfur, ASTM D3185-1A
 100 PartsPolymer, ASTM D3185-1A
 3 PartsZinc oxide, ASTM D3185-1A
 50 PartsCarbon black IRB8, ASTM D3185-1A
Total extractables31.8 percentASTM D5774

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Synthos BUNA™ SB 1502 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Synthos BUNA™ SB 1723 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Synthos BUNA™ SB 1500 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Synthos SPRINTAN™ SLR 4601 Solution Styrene Butadiene Rubber (S-SBR)

PDWST238 / 142447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.