MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxtral™ H1025 Performance Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.

Availability: Europe

Features:

  • Ductile
  • Good UV Resistance
  • High Flow
  • High Scratch Resistance
  • Low Temperature Impact Resistance
  • Paintable
Uses:
  • Automotive Applications
  • Automotive Bumper
  • Automotive Exterior Trim
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 230 °C
24 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 15.0 MPa2180 psiISO 527-2/50
Flexural Modulus 1.05 GPa152 ksiChord, 0.079 in/min; ISO 178
Izod Impact, Notched (ISO) 52.5 kJ/m²25.0 ft-lb/in²ISO 180/A
Impact Test 27.0 J19.9 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 59.4 µm/m-°C
@Temperature -30.0 - 100 °C
33.0 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 47.2 °C117 °FISO 75-2/Af

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zenite® 6330 BK010 LCP (Extended Tabular Temperature Data)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C)
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1025
FloMet 17-4PH Stainless Steel, Heat Treated (H-900)
Latitude Manufacturing PowderFlo® 17-4PH Stainless Steel Metal Injection Molding Compound

PEX99392 / 175628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.