MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical 40 AF Flame Retardant HIPS  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VTR, monitors, computers and other electrical electronic parts requiring flame retard

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength, Yield 26.5 MPa3840 psi50 mm/min; ASTM D638
Elongation at Break 60 %60 %50 mm/min; ASTM D638
Flexural Yield Strength 41.2 MPa5980 psi15 mm/min; ASTM D790
Flexural Modulus 2.20 GPa319 ksi15 mm/min; ASTM D790
Izod Impact, Notched  0.780 J/cm
@Thickness 6.35 mm
1.46 ft-lb/in
@Thickness 0.250 in
ASTM D256
 1.13 J/cm
@Thickness 3.17 mm
2.12 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secUL Rating PLC 6 (60-120 sec)
Comparative Tracking Index 250 - 400 V250 - 400 VUL Rating PLC 2
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secUL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsUL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minUL Rating PLC 1 (10-25.4 mm/min)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
@Thickness 12.7 mm
171 °F
@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 95.0 °C203 °F1000 g; ASTM D1525
Flammability, UL94  V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Descriptive Properties
IEC 707 FlammabilityFVO mm/min.1/16 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical HIPS 65IHE PS, Impact Modified
LG Chemical HIPS 405AF PS, Flame Retardant
LG Chemical HIPS 501S PS, Impact Modified
LG Chemical 401 AF Flame Retardant HIPS
INEOS Styrolution Terluran® HH-106 Q109 Colored ABS

PLAZ78 / 50336

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.