MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Terluran® HH-106 Q109 Colored ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in
Melt Flow 7.35 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.35 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 102 MPa
@Load 36.5 kg,
Time 30.0 sec
14800 psi
@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 51.0 MPa7400 psi50mm/min; ISO 527-1/-2
Elongation at Break 9.0 %9.0 %Nominal; ISO 527-1/-2
Elongation at Yield 3.0 %3.0 %50mm/min; ISO 527-1/-2
Tensile Modulus 2.40 GPa348 ksiISO 527-1/-2
Flexural Strength 72.0 MPa10400 psiISO 178
Izod Impact, Notched 2.20 J/cm4.12 ft-lb/inASTM D256
Izod Impact, Notched (ISO)  7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 19.0 kJ/m²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 19.0 J/cm²
@Temperature 23.0 °C
90.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Strength 39.0 kV/mm991 kV/inK20/P50; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 - 110 µm/m-°C
@Temperature 23.0 - 80.0 °C
44.4 - 61.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 85.0 °C185 °F
Deflection Temperature at 0.46 MPa (66 psi) 111 °C232 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 106 °C223 °FISO 75
Vicat Softening Point 106 °C223 °FVST/B/50; ISO 306
 115 °C239 °FVST/A/50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 270 °C446 - 518 °FInjection Molding
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °FInjection Molding
Drying Temperature 80.0 °C176 °FPre-drying
Dry Time 2 - 4 hour2 - 4 hourPre-drying
 
Descriptive Properties
ColorBlack 10351
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
INEOS Styrolution Novodur® 4000PG ABS
LG Chemical 40 AF Flame Retardant HIPS
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding

PBASG0613 / 132246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.