MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

FKuR Kunststoff Bio-Flex® F 9533 PLA Blend
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Bio-Flex® F 9533 has been designed especially for injection molding applications. Ideal for molding, a result of its excellent flow characteristics, its mechanical properties are comparable to conventional polystyrene (PS). Furthermore Bio-Flex® F 9533 is biodegradable with a high percentage of renewable resource raw material content. Biodegradable compound suitable for injection molding application. The biobased carbon content (BCC) is > 85 % (calculated).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Melt Flow 22 - 28 g/10 min
@Load 2.16 kg,
Temperature 190 °C
22 - 28 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 31.0 MPa4500 psiISO 527-1, ISO 527-2
Tensile Strength, Ultimate 50.0 MPa7250 psiISO 527
Elongation at Break 6.6 %6.6 %ISO 527
Modulus of Elasticity 4.60 GPa667 ksiISO 527
Flexural Strength 50.0 MPa
@Strain 3.5 %
7250 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 4.90 GPa711 ksiISO 178
Flexural Strain at Break 3.6 %3.6 %ISO 178
Charpy Impact Unnotched 3.45 J/cm²
@Temperature 23.0 °C
16.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1 eU
Charpy Impact, Notched 0.260 J/cm²
@Temperature 23.0 °C
1.24 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1 eA
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 155 °C>= 311 °FISO 3146-C
Vicat Softening Point 63.0 °C145 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FKuR Kunststoff Bio-Flex® F 7510 PLA Blend
FKuR Kunststoff Bio-Flex® FX 1803 Compostable PLA Blend
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA
FKuR Kunststoff Bio-Flex® F 6514 PLA Blend
GEHR Plastics ECOGEHR® PLA-N Polylactic Acid

PFKUR919 / 192744

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.