Bio-Flex® F 9533 has been designed especially for injection molding applications. Ideal for molding, a result of its excellent flow characteristics, its mechanical properties are comparable to conventional polystyrene (PS). Furthermore Bio-Flex® F 9533 is biodegradable with a high percentage of renewable resource raw material content. Biodegradable compound suitable for injection molding application. The biobased carbon content (BCC) is > 85 % (calculated). |