MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C61800
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Fabrication by hot forging and hot pressing.

Applications: bushings, bearings, corrosion resistant applications, welding rods.

Available as rod.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.65 g/cc0.276 lb/in³C62300
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 552 - 586 MPa80100 - 85000 psi
Tensile Strength, Yield 269 - 293 MPa39000 - 42500 psiDepending on temper
Elongation at Break 28 %28 %in 50 mm.
Tensile Modulus 117 GPa17000 ksi
Machinability 40 %40 %UNS C36000 (free-cutting brass) = 100%
Forgeability 50 %50 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000130 ohm-cm0.0000130 ohm-cm13% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 5.33 W/m-K37.0 BTU-in/hr-ft²-°F
Melting Point 1040 - 1045 °C1904 - 1913 °F
Solidus 1040 °C1904 °F
Liquidus 1045 °C1913 °F
Annealing Point 593 - 649 °C1100 - 1200 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10 %10 %
Copper, Cu 89 %89 %
Iron, Fe 1.0 %1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C61900
Copper, UNS C62500
8% Aluminum Bronze, UNS C61000
Copper, UNS C43500
Copper, UNS C61500

MC61800b1 / 11600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.