MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C61800
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Fabrication by hot forging and hot pressing.

Applications: bushings, bearings, corrosion resistant applications, welding rods.

Available as rod.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.65 g/ccC62300
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 552 - 586 MPa
Tensile Strength, Yield 269 - 293 MPaDepending on temper
Elongation at Break 28 %in 50 mm.
Tensile Modulus 17000 ksi
Machinability 40 %UNS C36000 (free-cutting brass) = 100%
Forgeability 50 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000130 ohm-cm13% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 37.0 BTU-in/hr-ft²-°F
Melting Point 1904 - 1913 °F
Solidus 1904 °F
Liquidus 1913 °F
Annealing Point 1100 - 1200 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 10 %
Copper, Cu 89 %
Iron, Fe 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C61900
Copper, UNS C62500
8% Aluminum Bronze, UNS C61000
Copper, UNS C43500
Copper, UNS C61500

MC61800b1 / 11600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.