MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tra-Con Tra-Bond F175 One-Part UV Curing Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND F175 is a clear, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure with ultraviolet light is desired. It is also recommended for electronic applications as it has very low ionic impurities. TRA-BOND F175 is a low viscosity system with a highly unique chemistry which produces very little shrinkage upon cure. It is an excellent choice for high humidity environments or applications requiring thermal cycling. HANDLING: TRA-BOND F175 should be stored with an air space to ensure maximum stability. Do not purge with nitrogen.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccMixed
Viscosity 2100 cP
@Temperature 25.0 °C
2100 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature 20.0 °C
72.2 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 11.0 °C51.8 °FUltimate Tg
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0167 min0.000278 hour400 W/inch @ 1"
 0.0667 min0.00111 hour400 W/inch @ 6"
 0.750 min0.0125 hour9 mW/inch @ 1"
 
Descriptive Properties
Color Light Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond F175T One-Part Thixotropic UV Curing Adhesive
Dymax 9-20558 Conformal Coating
Dymax 914-A Strain Relief, Wire and Parts Tacking Adhesive
Dymax 912 Strain Relief, Wire and Parts Tacking Adhesive
Dymax 910 Strain Relief, Wire and Parts Tacking Adhesive

PTRAC242 / 71170

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.