MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® XE 4071 nat PA612-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Product description: Grilamid XE 4071 NATURAL is an unreinforced impact modified high viscosity polyamide 612 (PA612) extrusion grade with superior hydrolysis and heat resistance. Compared to standard Grilamid grades XE 4071 NATURAL exhibits an improved resistance when exposed to water/glycol mixtures as found in automotive coolant fluids. Furthermore it is highly resistant to heat, automotive fluids and chemicals in general.

Grilamid XE 4071 NATURAL has been developed for use in the cooling / heating system of vehicles. One particular application is the use as outer layer material of the ECOSYS tube solution. Grilamid XE 4071 NATURAL is suitable for other demanding automotive tubings too. ECOSYS (= EMS Cooling System) is the designation of flexible partially corrugated multilayer tubes developed by EMSGRIVORY for automotive heating and cooling systems.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³Dry; ISO 1183
Water Absorption 2.7 %2.7 %Sim. to ISO 62
Moisture Absorption 1.20 %1.20 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.030 cm/cm0.030 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 70.0 MPa10200 psiConditioned; ISO 2039-1
 100 MPa14500 psiDry; ISO 2039-1
Tensile Strength, Yield 40.0 MPa5800 psiConditioned; ISO 527-1/-2
 50.0 MPa7250 psiDry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %Dry; ISO 527-1/-2
 20 %20 %Conditioned; ISO 527-1/-2
Tensile Modulus 1.20 GPa174 ksiConditioned; ISO 527-1/-2
 2.00 GPa290 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 40.0 kV/mm1020 kV/inDry; IEC 60243-1
 40.0 kV/mm1020 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 160 µm/m-°C88.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
Melting Point 210 °C410 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 120 - 140 °C248 - 284 °FLong Term; ISO 2578
 160 °C320 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Automotive electr. and electronics, lighting
 Compressed air systems
 Cooling and climate control
 Hydraulic systems
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingOther Extrusion
 Profile Extrusion
Product AttributesHigh viscosity
 Hydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsamid® DMVO PA612
EMS-Grivory Grilamid® 2D 20 nat PA612
EMS-Grivory Grilamid® L 25 Z PA12-I
Teknor Apex Chemlon 253 H Nylon 6, Impact Modified
EMS-Grivory Grilamid® 2D 25 W 20 HL X black 9992 PA612-I

PGRH122 / 156831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.