MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® 2D 25 W 20 HL X black 9992 PA612-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Grilamid 2D 25 W 20 HL X black 9992 are:
  • High strength, high burst pressure (tube)
  • High heat resistance
  • Significantly lower water absorption compared to standard polyamides
  • Good chemical and hydrolysis resistance
  • Low density
  • Easy processing
Grilamid 2D 25 W 20 HL X black 9992 has been developed for media lines in passenger cars and trucks. Thanks to its excellent heat resistance it is particularly suitable for diesel, air brake, cooling, oil and hydraulic tubes. The product is not recommended for direct permanent contact with gasoline. One particular application is the use as outer layer of multilayer ECOSYS coolant tubes. ECOSYS (EMS Cooling System) is the designation for tube solutions developed by EMS-GRIVORY for automotive heating and cooling systems.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³Dry; ISO 1183
Water Absorption 2.1 %2.1 %Sim. to ISO 62
Moisture Absorption 0.900 %0.900 %Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 30.0 MPa4350 psiConditioned; ISO 2039-1
 39.0 MPa5660 psiDry; ISO 2039-1
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Conditioned; ISO 527-1/-2
Tensile Modulus 0.380 GPa55.1 ksiConditioned; ISO 527-1/-2
 0.550 GPa79.8 ksiDry; ISO 527-1/-2
50% Modulus  25.0 MPa
@Strain 50 %
25.0 MPa
@Strain 50 %
Conditioned; ISO 527-1/-2
 30.0 MPa
@Strain 50 %
30.0 MPa
@Strain 50 %
Dry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 ohm-cm1.00e+7 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Strength 37.0 kV/mm940 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 250 µm/m-°C139 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
Melting Point 210 °C410 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C176 - 230 °FLong Term; ISO 2578
 150 °C302 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AdditivesPlasticizer
AutomotiveAir intake systems
 Compressed air systems
 Cooling and climate control
 Fuel systems
 Hydraulic systems
 Powertrain and Chassis
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
ProcessingOther Extrusion
 Profile Extrusion
Product AttributesFlexible
 High viscosity
 Hydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Light stabilized or stable to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® 2D 25 W 20 X nat PA612-I
DuPont Mobility and Materials Zytel® LC6159 BK554 PA612
EMS-Grivory Grilamid® 1SBVX-30H LDS black PA1010-GF30
EMS-Grivory Grilamid® 1S XE 4224 nat PA1010
EMS-Grivory Grilon® BT 40 Z PA6

PGRH009 / 156718

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.