MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics IFB Insulation Range JM™ 23 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: JM™ IFB ranges, manufactured via cast process, are market leaders in applications such as Petrochemical and Ceramics where the ability to operate in environments above 1000°C (1800°F) is critical. With low thermal conductivity, due to the unique manufacturing process, the IFB’s deliver the erfect balance of low density and homogenous porosity. Our IFB range delivers big energy savings for many markets and our global manufacturing footprint enables Morgan to meet your regional and global application demands.

Applications: While commonly used in back-up insulation they may also be used as hot face in selected applications. Overall uses include:

  • Aluminium (anode bake furnaces, primary electrolytic cells, holding and melting furnaces and secondary re-melt furnaces)
  • Petrochemical (kilns, flues, refining vessels and heaters and reactor chambers)
  • Iron and steel industry (heat treatment and galvanising)
  • Coke and iron making (blast furnaces, hot blast stoves, hot blast and bustle main)
  • Hobby and laboratory kilns
  • Ceramic industry (including kilns for domestic use)
  • Glass industry

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.480 g/cc0.0173 lb/in³ASTM C-133
Deformation 0.10 %
@Temperature 1100 °C,
Time 5400 sec
0.10 %
@Temperature 2010 °F,
Time 1.50 hour
Hot Load Strength, 0.069 MPa
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00100 GPa0.145 ksi
Compressive Strength 1.20 MPa174 psiCold Crushing Strength; ASTM C-133
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.88 J/g-°C0.450 BTU/lb-°FASTM C-182
Thermal Conductivity  0.120 W/m-K
@Temperature 400 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-182
 0.140 W/m-K
@Temperature 600 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-182
 0.170 W/m-K
@Temperature 800 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C-182
 0.190 W/m-K
@Temperature 1000 °C
1.32 BTU-in/hr-ft²-°F
@Temperature 1830 °F
ASTM C-182
Shrinkage 0.20 %
@Treatment Temp. 1230 °C,
Time 86400 sec
0.20 %
@Treatment Temp. 2250 °F,
Time 24.0 hour
soak; ASTM C-210
 
Component Elements PropertiesMetricEnglishComments
Al2O3 37 %37 %
CaO 15.2 %15.2 %
Fe2O3 0.70 %0.70 %
Other 1.4 %1.4 %Na2O+K2O+MgO
SiO2 44.4 %44.4 %
TiO2 1.2 %1.2 %
 
Descriptive Properties
Classification Temperature (°C)1260
Reversible Linear Thermal Expansion Max (%)0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics IFB Insulation Range JM™ 23-400 Thermal Ceramic
Morgan Advanced Ceramics Kaowool Millboard 822 Thermal Ceramic
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 304SS Washers and Studs
Morgan Advanced Ceramics Insulite H Thermal Ceramic
Morgan Advanced Ceramics IFB Insulation Range TJM ™ 23 Thermal Ceramic

CMORF6166 / 202950

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.