MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES HiFill® PA6 CF30 30% Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by Weight

Appearance: Black and Natural Color

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 3.17 mm
0.0060 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Yield 214 MPa31000 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Flexural Strength 310 MPa45000 psiASTM D790
Flexural Modulus 17.2 GPa2500 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 23.4 µm/m-°C13.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 216 °C420 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese CoolPoly® E3607 Thermally Conductive Polyamide (PA6)
Celanese CoolPoly® E3603 Thermally Conductive Polyphthalamide (PPA)
Celanese CoolPoly® D5110 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
Akro-Plastic Akromid® C3 GF 60 1 black (4353) PA66 + PA6, Conditioned, 60% Glass Filled

PTPC0153 / 136091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.