MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES HiFill® PA6 CF30 30% Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by Weight

Appearance: Black and Natural Color

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D792
Water Absorption 1.0 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Yield 31000 psiASTM D638
Elongation at Break 1.5 %ASTM D638
Flexural Strength 45000 psiASTM D790
Flexural Modulus 2.50e+6 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 13.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 420 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 410 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese CoolPoly® E3607 Thermally Conductive Polyamide (PA6)
Celanese CoolPoly® E3603 Thermally Conductive Polyphthalamide (PPA)
Celanese CoolPoly® D5110 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
Akro-Plastic Akromid® C3 GF 60 1 black (4353) PA66 + PA6, Conditioned, 60% Glass Filled

PTPC0153 / 136091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.