MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Injection Rate: Fast

Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D792
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 858515 seconds; ASTM D2240
Tensile Strength at Break 16.5 MPa2400 psiASTM D412
Tensile Stress at Strain 7.93 MPa
@Strain 100 %
1150 psi
@Strain 100 %
ASTM D412
Elongation at Break 400 %400 %ASTM D412
Tear Strength 70.1 kN/m400 pliASTM D624
Compression Set 60 %
@Temperature 125 °C,
Time 79200 sec
60 %
@Temperature 257 °F,
Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 173 - 213 °C344 - 416 °F
Middle Barrel Temperature 179 - 219 °C354 - 426 °F
Front Barrel Temperature 184 - 224 °C364 - 436 °F
Nozzle Temperature 190 - 230 °C374 - 446 °F
Zone 1 166 - 204 °C330 - 400 °F
Zone 2 171 - 210 °C340 - 410 °F
Zone 3 177 - 216 °C350 - 420 °F
Zone 5 182 - 221 °C360 - 430 °F
Die Temperature 190 - 227 °C374 - 440 °F
Melt Temperature 190 - 230 °C374 - 446 °FProcessing Temperature
Mold Temperature 35.0 - 60.0 °C95.0 - 140 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 120 rpm50 - 120 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer
ExxonMobil Santoprene® 8221-85M300 Thermoplastic Elastomer

PTEKNO889 / 129070

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.