MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M20 266°F (130°C) Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: M20 was designed to meet need for high temperature performance combined with a low energy cure cycle. Suitable for aircraft primary and secondary structures, and composite repair.

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 175 MPa25400 psiISO 604
Compressive Modulus 3.06 GPa444 ksiISO 604
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 150 °C302 °Fdmta

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® M27 248°F (120°C) Curing Epoxy Matrix
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix
Hexcel® HexPly® M18/1 180°C Curing Epoxy Matrix
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix

PHEXC161A / 98632

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.