ELITE™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, this resin provides excellent extensibility for high yields on regular loads. ELLITE™ 5230G resin complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2a. Information provided by Dow |