MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ELITE™ 5230G Enhanced Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: ELITE™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, this resin provides excellent extensibility for high yields on regular loads. ELLITE™ 5230G resin complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2a.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.916 g/ccASTM D792
Thickness 0.800 mil
Melt Flow 4.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1385 psiASTM D882
Film Tensile Strength at Yield, TD 1240 psiASTM D882
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 630 %ASTM D882
Elongation, Ultimate 330 %on-pallet testing; Dow Method
Impact 9.0[lbf]; Puncture Resistance Force; Dow Method
 47[N]; Puncture at 250% pre-stretch; on-pallet testing; Dow Method
Puncture Energy 33.0 in-lbDow Method
Elmendorf Tear Strength MD 360 gASTM D1922
Elmendorf Tear Strength TD 520 gASTM D1922
Elmendorf Tear Strength, MD 450 g/milASTM D1922
Elmendorf Tear Strength, TD 650 g/milASTM D1922
Dart Drop Test 630 gMethod B; ASTM D1709
Film Tensile Strength at Break, MD 5900 psiASTM D882
Film Tensile Strength at Break, TD 5200 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 122 °CDow Method (DSC)
 
Optical PropertiesOriginal ValueComments
Haze 0.50 %ASTM D1003
Gloss 95 %45°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ATTANE™ 4404G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer
Dow ELITE™ 5220G Enhanced Polyethylene Resin
Dow ELITE™ 5400G Enhanced Polyethylene Resin
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin
ExxonMobil Exceed™ m 3518.PA Cast Premium Cast Film Resin

PDOW1325 / 30543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.