MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

DuPont Mobility and Materials VTR 8500 (GLT-S) 8500 Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton® VTR-8500 is a developmental peroxide cured polymer intended to be an upgrade to Viton® GLT. VTR-8500 utilizes an Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:
  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to GLT and GLT 305
  • Shows improved mold flow, less shear sensitivity, and lower extruder die swell for a ~65 Mooney FKM
  • Shows excellent physical properties with high elongation in either the original or aging tests
  • Shows similar to improved heat, fluids, and low temperature resistance compared to GLT
  • Shows excellent compression set resistance with little (2 hr at 232°C ) or no postcure

It is recommended if mixing in an internal mixer to use at least a 70% load factor. The recommended process aid for VTR-8500 is 0.5 phr of Armeen® 18D.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 66
@Temperature 121 °C
66
@Temperature 250 °F
ML-10 (gum)-Akron data
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 17.8 MPa2580 psiCured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Yield 0.600 MPa87.0 psi10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 267 %267 %Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 3.60 MPa
@Strain 100 %
522 psi
@Strain 100 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 11 %
@Temperature 200 °C
11 %
@Temperature 392 °F
Method B, O-rings 22 hr at 200°C (Cured 7 min at 177°C and Post Cured 2 hr at 232°C)
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -31.4 °C-24.5 °FTR-10
Glass Transition Temp, Tg -32.9 °C-27.2 °FDSC
 
Descriptive Properties
Formulation as Tested100Viton® GLT
 3Zinc Oxide
 3Diak™ 7
 3Luperox® 101-XL
 30N990 Carbon Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured
Seals Eastern 5724 Fluorocarbon-Elastomer
Chemours Viton® F-601C Fluoroelastomer (FKM)
Greene Tweed Fluoroelastomer 742 FKM
Seals Eastern 5725 Fluorocarbon-Elastomer

PDVDA44 / 34013

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.