Description: ANDEROL PQ Assembly Lube grease is made from pure white mineral oil and additives to produce a general purpose food grade grease for lubrication of enclosed bearings, o-rings and other devices where incidental food contact is possible. Information provided by ConocoPhillips. Anderol® is a registered trademark of The Anderol Company. |