MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Anderol ANDEROL® PQ Assembly Lube Premium Quality White Mineral Oil Food Grade Grease, NLGI 1.5  (discontinued **)
Categories: Fluid; Lubricant; Aluminum Gellant; Organic Soap Gellant; White Mineral Oil (WMO)

Material Notes: Description: ANDEROL PQ Assembly Lube grease is made from pure white mineral oil and additives to produce a general purpose food grade grease for lubrication of enclosed bearings, o-rings and other devices where incidental food contact is possible.

Information provided by ConocoPhillips.

Anderol® is a registered trademark of The Anderol Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 98Viscosity Index (base oil property)
Kinematic Viscosity at 40°C (104°F) 103 cStBase Oil Property
Kinematic Viscosity at 100°C (212°F) 11.5 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Penetration 246.5 - 347.5Worked 10,000 Strokes, 77°F; ASTM D-217
Penetration P(60), 1/10 mm 297ASTM D-217, 77°F
 
Thermal PropertiesOriginal ValueComments
Pour Point 10.0 °FBase Oil Property
Dropping Point 500 °F
 
Descriptive Properties
ColorClear/light yellow
TextureSmooth, tacky
ThickenerAluminum Complex

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Applied Silicone 40073 MDM Silicone Fluid, (350) Medical Grade
Nye Lubricants PG-44A Grease
Nye Lubricants 675A Grease
Nye Lubricants 675 Grease
Silikony Polskie Silpasta A Silicone Paste

WCON315 / 75352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.