MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oceanchem Group Antioxidant 168
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C42H63O3P

Cas No.: 31570-04-4

Characteristics and Uses: This product is an excellent antioxidant namely applied to polyethylene, polypropylene, polyoxymethylene, ABS resin, PS resin, PVC, engineering plastics, binding agent, rubber, petroleum etc. for product polymerization.

Storing and Packing: This product is nontoxic, inflammable, noncorrodible and stable in storing, packed in cardboard pail lined with plastic bags with the net capacity of 25 kg per pail.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 182 - 185 °C360 - 365 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  >= 97 %
@Wavelength 425 nm
>= 97 %
@Wavelength 425 nm
10g/100ml Toluene; clarified at room temperature
 >= 97 %
@Wavelength 500 nm
>= 97 %
@Wavelength 500 nm
10g/100ml Toluene; clarified at room temperature
 
Descriptive Properties
AppearanceWhite crystalline powder
CAS Number31570-04-4
Chemical NameTri(2,4-Tertbutylphenyl)Phosphorite
Content (%)>99.0
Ethyl Acetate (%)114% Ethane (20°C, W/W)
 36Cycloehexane
Methanol (%)<0.01Water
 36Dichloromethane
Molecular FormulaC42H63O3P
Solubility0.01%Acetone
 34%Benzene
 36%Chloroform

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman 9921P PET Film
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 5.0 PHR Wacker HDK N20 Filler
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler
Suqian Unitechem UV-P
Suqian Unitechem 2,2,6,6-tetramethyl-4-piperidinol

POCEAN54 / 104258

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.