MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

M. Holland Company MTEGRITY™ HD400 HDPE, Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Features: High ESCR (Stress Crack Resist.), Medium Flow, High Impact Resistance, Narrow Molecular Wt. Dist.

Uses: Automotive Applications, Closures, Containers, Toys

Approvals: FDA 21 CFR 177.1520 and ASTM D 1248, III, Class A, Cat. 2

Processing Method: Injection Molding

Information provided by M. Holland.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D4883
Melt Flow 11.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.5 MPa3700 psiASTM D638
Elongation at Break 700 %700 %ASTM D638
Flexural Modulus 1.24 GPa180 ksi3% Tangent; ASTM D790
 0.965 GPa
@Strain 3 %
140 ksi
@Strain 3 %
Secant; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °F
Vicat Softening Point 123 °C253 °FASTM D1525
Brittleness Temperature -70.6 °C-95.0 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
M. Holland Company MTEGRITY™ HD100 HDPE, Copolymer
M. Holland Company MTEGRITY™ HD300 HDPE, Copolymer
M. Holland Company MTEGRITY™ HD145 HDPE
ExxonMobil Paxon™ BA50-100 Blow Molding Resin
Chevron Phillips Marlex® 9518H High Density Polyethylene, Blow Molding

PMH024 / 52957

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.