MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® 9518H High Density Polyethylene, Blow Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: This gas phase, high molecular weight, homopolymer is tailored for lightweight blow molded applications that:
  • Require excellent stiffness to ESCR ratio
  • Require good melt strength
  • Are durable and recyclable for sustainability

Typical blow molded applications for 9518H include:

  • Household and industrial chemical containers
  • Industrial containers / Large parts

This resin meets these specifications:

  • ASTM D4976 - PE 245
  • FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)

Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.962 g/cc0.962 g/ccASTM D1505
ESCR 100% Igepal® 24 hour24 hourCondition B, F50; ASTM D1693
Melt Flow 0.34 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.34 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.0 MPa4640 psi2 in/min, Type IV bar; ASTM D638
Elongation at Break >= 500 %>= 500 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.48 GPa215 ksiTangent; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FType A clamp, Type I Specimen; ASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® EHM 6004 High Density Polyethylene, Blow Molding
Petromont 8001 High Density Polyethylene Resin
Braskem BU004 Blow Molding High Density Polyethylene
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin

PCHEVC910 / 130393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.