MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Biomax® PTT 1100  (discontinued **)
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic

Material Notes: DuPont™ Biomax® PTT 1100 resin can help reduce your packaging footprint on the environment while also offering superior aesthetics and resistance to most formulations. Plastic made from petrochemicals deliver high performance in packaging, but use depletable petroleum resources as their primary feedstock. DuPont™ Biomax® PTT is a solution to provide high-performance plastic packaging made from partially renewable feedstocks. Biomax® PTT 1100 contains up to 37% renewably sourced content by weight and injection molds similarly to PBT.
    Environmental value proposition:
  • Partially renewably-sourced material solution which contributes positively to decreasing greenhouse gas emissions over a product life cycle
  • Regrind can be reused in standard in-plant processes
    Performance attributes:
  • Glossy surface to provide attractive aesthetics
  • Excellent resistance to common personal care & cosmetic formulations
  • Good colorability
  • Naturally opaque to translucent
  • High strength
DuPont™ Biomax® PTT is a unique polymer based on 1,3 bio-propanediol, a monomer originating from common agricultural sources, such as corn or sugar beets.
    Uses:
  • Cosmetic Packaging
  • Packaging
Appearnce: Natural, Off-White and Opaque

Processing Method: Injection Molding

    Availability:
  • Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
  • South America
Information provided by DuPont™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Melt Flow 35 g/10 min
@Temperature 250 °C
35 g/10 min
@Temperature 482 °F
150 ppm
 
Thermal PropertiesMetricEnglishComments
Melting Point 228 °C442 °F
Glass Transition Temp, Tg 55.0 °C131 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Sorona® 3030G BK001 PTT-GF30
DuPont Mobility and Materials Sorona® 3301 NC010 PTT
Overview of materials for Polytrimethylene Terephthalate (PTT)
RTP Company RTP 4700 Polytrimethylene Terephthalate (PTT), Base Resin
Celanese GUR® HOSTALLOY 731 Injection Molding Grade Polyethylene Resin

PDUP972a / 133225

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.