System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese GUR® HOSTALLOY 731 Injection Molding Grade Polyethylene Resin
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Injection Molded
Material Notes:
Description:
General purpose injection molding grade. Designed to offer the good balance of performance and processability. Good wear, low COF and excellent low temperature impact.
Information provided by Celanese Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.950
g/cc
0.0343
lb/in³
ASTM D792
Water Absorption
0.00 %
0.00 %
24 hour immersion; ASTM D570
Viscosity Test
3800
cm³/g
38.0
dl/g
ISO 307, 1157, 1628
Linear Mold Shrinkage
0.020
-
0.030
cm/cm
0.020
-
0.030
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.020
-
0.030
cm/cm
0.020
-
0.030
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
68
68
ASTM D2240
Tensile Strength at Break
28.3
MPa
4100
psi
ASTM D638
Tensile Strength, Yield
34.5
MPa
5000
psi
ASTM D638
Elongation at Break
100 %
100 %
ASTM D638
Elongation at Yield
22 %
22 %
ASTM D638
Flexural Modulus
1.17
GPa
170
ksi
ASTM D790
Izod Impact, Notched
NB
NB
ASTM D256
9.61
J/cm
@Temperature -40.0 °C
18.0
ft-lb/in
@Temperature -40.0 °F
ASTM D256
Coefficient of Friction, Dynamic
0.070 - 0.090
0.070 - 0.090
vs steel; Internal
Taber Abrasion, mg/1000 Cycles
1.7
1.7
ASTM D4060
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
81.0
°C
178
°F
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer
BASF Petra® 130 30% Glass Filled PET
PHCV44 / 45884
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.