MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman AVALON® 95 AHT Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: AVALON® AHT TPUs are colorless, UV resistant and offer high transparency – even where parts need to be thick. With hardness levels ranging from 90 to 95 Shore A, AVALON® AHT is ideal for consumer applications such as footwear soiling and protective cover for mobile phones and tables.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ISO 868
Hardness, Shore D 4848ISO 868
Tensile Strength at Break 47.0 MPa6820 psiISO 37
Elongation at Break 390 %390 %ISO 37
Tear Strength 118 kN/m673 pliISO 34B
Abrasion 2828mm3; ISO 4649

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Covestro Baytec® P-132 Polyurethane
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer

PHUQ179 / 159552

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.